Engineering Work in Towns and CitiesM.C. Clark publishing Company, 1908 - 502페이지 |
기타 출판본 - 모두 보기
자주 나오는 단어 및 구문
angle asphalt beam bending moment blocks bottom brick building calculated catch basins cement cent center of gravity city engineer clean Coal column concrete contract contractor or contractors corner cost cubic cubic foot curb curve depth diagram diameter distance drain drawer drawings earth edge elevations equal feet field book filed filled foot formula grade gravel gutter horizontal Improvements inches intersection iron Job Book joints laid LAUGHLIN HAND BOOK layer length macadam manholes marked material measure method mixed modulus of elasticity mortar neutral axis ordinance parabola pavement paving pipe placed plats Portland cement pounds proper protractor radius radius of gyration records reinforced concrete roads roadway sand sewer sheets side sidewalk span specifications square stadia stakes steel stone street stress surface survey tamped thickness town trench triangle vertical wall weight width writer
인기 인용구
148 페이지 - ... shall be punished by a fine of not less than five dollars ($5.00) nor more than one hundred dollars...
157 페이지 - Bidders must satisfy themselves, by personal examination of the location of the proposed work, and by such other means as they may prefer, as to the...
6 페이지 - The true strong and sound mind is the mind that can embrace equally great things and small.
229 페이지 - A third pat is exposed in any convenient way in an atmosphere of steam, above boiling water, in a loosely closed vessel for five hours.
228 페이지 - It shall develop initial set in not less than thirty minutes, but must develop hard set in not less than one hour, nor more than ten hours.
255 페이지 - Another approved method, which may be permitted at the option of the Engineer in charge, is to spread the sand, then the cement and mix dry, then the gravel or broken stone; add water and mix thoroughly as above.
228 페이지 - Pats of neat cement about three inches in diameter, one-half inch thick at center, tapering to a thin edge, shall be kept in moist air for a period of twenty-four hours. (a) A pat is then kept in air at normal temperature. (b) Another is kept in water maintained as near 70° F.
226 페이지 - The cement shall be stored in such a manner as to permit easy access for proper inspection and identification of each shipment, and in a suitable weather-tight building which will protect the cement from dampness.